COMPARISON OF CYCLIC FATIGUE RESISTANCE OF ONE CURVE, HYFLEX EDM, WAVEONE GOLD AND RECIPROC BLUE NICKELTITANIUM ROTARY FILES AT INTRA-CANAL TEMPERATURE
dc.contributor.author | Yılmaz, Koray | |
dc.contributor.author | Özyürek, Taha | |
dc.contributor.author | Uslu, Gülşah | |
dc.date.accessioned | 2025-01-27T19:38:47Z | |
dc.date.available | 2025-01-27T19:38:47Z | |
dc.date.issued | 2019 | |
dc.department | Çanakkale Onsekiz Mart Üniversitesi | |
dc.description.abstract | Objectives: To compare the cyclic fatigue resistances of One Curve (OC), HyflexEDM (HEDM), WaveOne Gold (WOG), Reciproc Blue (RPC Blue), and nickeltitanium rotary files at intra-canal temperature (35°C).Materials and Methods: Twenty OC (25/.06), 20 HEDM (25/.08), 20 WOG(25/.07) and 20 RPC Blue (25/.08) files were tested for cyclic fatigue at intracanal temperature (35°C). All the instruments were rotated in artificial which weremade of stainless steel with an 60° angle of curvature and a radii of curvatures of5 mm until fracture occurred, and the time to fracture was recorded in secondsusing a digital chronometer and the number of cycles to fracture (NCF) for eachfile was calculated. The Kruskal-Wallis test was performed to statistically analyzethe data by using SPSS 21.0 software. The statistical significance level was set atp<.05.Results: NCF values revealed that the HEDM had the highest cyclic fatigueresistance at intracanal temperature (p<.05) and followed by WOG, RPC Blue andOC. The lowest NCF values were determined in the OC group and statisticallysignificant difference was observed between the OC group the other groups(p<.05). No statistically significant difference in the mean length of the fracturedfragments in curvature was evident for the instruments (p>.05).Conclusion: Within the limitations of the present in-vitro study, HEDMinstrument resisted static cyclic fatigue significantly more than RPC Blue, WOGand OC instruments. | |
dc.identifier.doi | 10.7126/cumudj.477218 | |
dc.identifier.endpage | 47 | |
dc.identifier.issn | 1302-5805 | |
dc.identifier.issn | 2146-2852 | |
dc.identifier.issue | 1 | |
dc.identifier.startpage | 42 | |
dc.identifier.trdizinid | 386023 | |
dc.identifier.uri | https://doi.org/10.7126/cumudj.477218 | |
dc.identifier.uri | https://search.trdizin.gov.tr/tr/yayin/detay/386023 | |
dc.identifier.uri | https://hdl.handle.net/20.500.12428/17373 | |
dc.identifier.volume | 22 | |
dc.indekslendigikaynak | TR-Dizin | |
dc.language.iso | en | |
dc.relation.ispartof | Cumhuriyet Dental Journal | |
dc.relation.publicationcategory | Makale - Ulusal Hakemli Dergi - Kurum Öğretim Elemanı | |
dc.rights | info:eu-repo/semantics/openAccess | |
dc.snmz | KA_TRD_20250125 | |
dc.subject | Diş Hekimliği | |
dc.subject | İmalat Mühendisliği | |
dc.title | COMPARISON OF CYCLIC FATIGUE RESISTANCE OF ONE CURVE, HYFLEX EDM, WAVEONE GOLD AND RECIPROC BLUE NICKELTITANIUM ROTARY FILES AT INTRA-CANAL TEMPERATURE | |
dc.type | Article |