Kaya, İsmetKoyuncu, SermetÇulhaoğlu, Süleyman2025-01-272025-01-2720080032-38611873-2291https://doi.org/10.1016/j.polymer.2007.12.010https://hdl.handle.net/20.500.12428/23529Polyazomethines including perylene units in the main chain were synthesized via polycondensation of diaminoperylene with aromatic dialdehydes. UV/vis, FT-IR, H-1 NMR, C-13 NMR and elemental analysis techniques were carried out for the characterization of the synthesized diaminoperylene, dialdehydes and polyazomethines including perylene units (PAM-PERs). The number-average molecular weight (M-n), weight-average molecular weight (M-w) and polydispersity index (PDI) values of PAM-PERs were determined by size exclusion chromatography (SEC). Thermal properties of PAM-PERs was determined by using TGA/DTA and DSC systems. The highest occupied molecular orbital (HOMO) and the lowest unoccupied molecular orbital (LUMO) energy levels, and electrochemical (E-g') and optical (E-g) hand gap values were calculated by using the results of cyclic voltammetry and UV/vis, respectively. Conductivity measurements of PAM-PERs were carried out with electrometer by using four-point probe technique. The conductivity was observed to be increased by doping agent iodine. (c) 2007 Elsevier Ltd. All rights reserved.eninfo:eu-repo/semantics/closedAccesspolyazomethinesperyleneconducting polymerSynthesis and characterization of novel polyazomethines containing perylene unitsArticle49370371410.1016/j.polymer.2007.12.010Q1WOS:0002537468000062-s2.0-38349191356Q1