Syntheses, structures and properties of novel oligo(azomethine ether)s containing or not chlorine atoms in the main chain

Yükleniyor...
Küçük Resim

Tarih

2009

Dergi Başlığı

Dergi ISSN

Cilt Başlığı

Yayıncı

Industrial Chemistry Research Inst

Erişim Hakkı

info:eu-repo/semantics/openAccess

Özet

New oligoazomethines were synthesized via polycondensation of aromatic diamines with one of two dialdehydes. Both dialdehydes, namely 4-({2-[(4-formylphenoxy)methyl]benzyl}oxy)benzaldehyde (2-FPMBB), and 4-({4-[(4-formylphenoxy)methyl]benzyl}oxy)benzaldehyde (4-FPMBB) were prepared from p-hydroxybenzaldehyde with o-xylenedibromide or p-xylenedibromide, respectively. Dialdehydes and oligomers were characterized by FT-IR, H-1 NMR and C-13 NMR methods. Size exclusion chromatography (SEC) technique was used to determine molecular weights and molecular weight distributions of synthesized oligomers. The thermal stability of oligomers was conducted by thermogravimetric analysis (TGA) and differential thermal analysis (DTA). The weight losses of oligoazomethines (O1, O2, O3 and O4) at 1000 degrees C were found to be 54.74, 46.27, 54.85 and 53.10% respectively. In all cases, the imine (-HC=N-) linkage is the first breaking group due to the high temperature. It can be seen from TGA that oligo(azomethine ether)s containing chlorine atoms have higher thermal stability at 1000 degrees C than O1 and O3 oligomers.

Açıklama

“Polimery” journal is an open access, peer-reviewed journal. All articles are published and distributed under a CC BY-NC-ND 4.0 Creative Commons license.

Anahtar Kelimeler

oligoazomethines, dialdehyde monomers, molecular weight distribution, thermal stability